Clean Rite has sealed brick pavers, travertine, and natural stone across Wesley Chapel and Pasco County since 2015. Florida's heavy summer rain is what washes joint sand out of paver driveways and pool decks, so the process starts by pressure washing out the old mildewed sand joints and re-sanding with SEK ASTM-C144 joint sand, not play sand or pool filter sand, for the rock solid joint stabilization that holds through the rainy season. Homeowners in communities like Angeline, Land O' Lakes, and Lutz choose between a natural-look matte finish with Trident Cyclone or a color-enhanced, joint-stabilizing seal with Trident Cat 5, so the finished surface matches the look they want rather than a one-size gloss.
The process, named out loud
Ask any paver quote to name their sand and their sealer. If they cannot, you have learned what you needed to know. I'm master certified by Trident, the maker of the sealer I use, and Trident has had me teach sealing to their other customers. Here is mine, the same sequence on every job:
- 1
Prep the surface honestly
Old silicone comes off along coping and hot tub lines. Failed sealer gets identified now, because sealing over a problem locks the problem in.
- 2
Pressure wash out the old joints
The mildewed, weed-seeded, washing-out sand comes OUT of the joints. Sealing over bad sand is how you get joints that stay rubbery and crumble.
- 3
Re-sand with SEK ASTM-C144 joint sand
The correct spec sand, in pearl or tan. Never play sand, pool filter sand, or blasting sand. This is where rock solid joint stabilization comes from.
- 4
Seal with the Trident finish you chose
Trident Cat 5 for a color-enhanced, joint-stabilizing seal, or Trident Cyclone for a natural matte look. Your surface, your call, explained before you decide.
Natural look or color enhanced. You choose.
Most companies roll one glossy product on everything. I carry two finishes because pavers and travertine do not all want the same look.
Trident Cyclone
Natural look, matte
- ✓Keeps the stone's dry, natural color
- ✓Matte surface, keeps more grip when wet
- ✓The usual choice for travertine and pool decks
- ✓Protection without announcing itself
Trident Cat 5
Color enhanced, joint stabilizing
- ✓Deepens color like the surface looks when wet
- ✓Two-part product that locks joint sand
- ✓The usual choice for driveways and patios
- ✓The richest version of your pavers' own color

How sealing goes wrong (and how I fix it)
Sealing fails in specific, visible ways. The surface turns white, cloudy, or hazy because moisture got trapped under the wrong product. The joints stay rubbery and wash out because the wrong sand went in, or the old sand never came out. Travertine yellows because someone rolled a film-forming sealer on a stone that needs to breathe.
Every one of those failures is a process shortcut, and every one costs more to undo than doing it right would have cost. When it has already happened, the fix is stripping the failed sealer and starting the process from bare, dry pavers. If your surface has already turned white or hazy, read why pavers turn white before anyone touches it again, especially anyone offering to reseal over it.

The three-year test
Anyone can make pavers look good the afternoon the sealer dries. The question is what the job looks like after three Florida rainy seasons. I went back to a job I sealed three years earlier, and the sand joints were still intact, ready for a freshen-up coat rather than a redo. In this climate a sealed surface typically wants another coat every couple of years, and when the joints held, that next coat is quick and clean.
That is the practical difference the sand spec and the two-part sealer make. The materials cost more. The job costs less over its life.

Where do you need sealing?
Straight answers
The questions I actually get, answered the way I answer them on the phone.
What sand do you use?
SEK ASTM-C144 joint sand, in pearl or tan. Never play sand, pool filter sand, or sand made for sand blasting. The spec matters: correct joint sand is what compacts into a stable joint and holds through Florida rain instead of washing out.
Will the joint sand wash out when it rains?
Not when the joints were done right. The failure you have seen or lived with comes from wrong sand or from new sand poured over old contaminated joints. My process washes the old joints out, re-sands with the correct spec, and stabilizes them with the seal. That is the rock solid joint stabilization the whole process is built around.
How long does paver sealing last in Florida?
Plan on a freshen-up coat roughly every two to three years in this climate. Sun, rain, and traffic set the exact pace. When the joints held, the re-coat is straightforward, and I have returned to a three-year-old job of my own with the sand joints still intact.
Why did my pavers turn white or cloudy after sealing?
Almost always moisture trapped under a sealer that could not breathe, common with cheap products or sealing done before the surface fully dried. The fix is stripping and resealing correctly, never another coat on top. The full explanation is on the why pavers turn white page.
Is a sealed pool deck slippery when wet?
It depends entirely on the finish. A glossy film can be slick; a natural matte finish like Trident Cyclone keeps more grip. On pool decks I walk you through that choice before anything gets applied.